化学科研者一站式服务平台
化合物简介
Palladium Hydroxide is a catalyst for hydrogenation reactions as well as in the synthesis of glycopeptides used in obtaining antibodies from autoimmune diseases.
基本信息
CAS:12135-22-7
中文别名:碳负载氢氧化钯;氢氧化钯/碳;氢氧化钯炭;
英文别名:Palladium Hydroxide;Palladium(II) hydroxide;palladium(2+),dihydroxide;
分子式:H2O2Pd
分子量:140.435
精确质量:139.909
Psa:46.12
Logp:-0.3536
中文别名:碳负载氢氧化钯;氢氧化钯/碳;氢氧化钯炭;
英文别名:Palladium Hydroxide;Palladium(II) hydroxide;palladium(2+),dihydroxide;
分子式:H2O2Pd
分子量:140.435
精确质量:139.909
Psa:46.12
Logp:-0.3536
编号系统
MDL号:MFCD00064599
PubChem号:24859831
EINECS号:235-219-2
PubChem号:24859831
EINECS号:235-219-2
物化性质
外观与性状:黑色粉末
沸点:100ºC at 760 mmHg
储存条件:Store in a tightly closed container. Store in a cool, dry, well-ventilated area away from incompatible substances.
蒸汽压:24.5mmHg at 25°C
沸点:100ºC at 760 mmHg
储存条件:Store in a tightly closed container. Store in a cool, dry, well-ventilated area away from incompatible substances.
蒸汽压:24.5mmHg at 25°C
安全信息
安全说明:S24/25
危险类别码:R11; R36/37/38
危险品运输编码:UN1325
危险类别:4.1
包装等级:III
危险品标志:F; Xi
危险类别码:R11; R36/37/38
危险品运输编码:UN1325
危险类别:4.1
包装等级:III
危险品标志:F; Xi
生产方法及用途
生产方法
30g氯化钯溶于43ml浓盐酸和570ml水中,加入68.6g活性炭,迅速搅拌并加热至60℃。在此混合物中加入31g粒状氢氧化钠,加入的速度以温度不超过80℃为宜。然后在混合物中加入6.6g固体碳酸氢钠,搅拌12h。滤出催化剂,用430ml水洗涤,再用430ml水和8.6ml乙酸的混合液洗涤。滤出催化剂,在65℃真空下干燥。在N2保护下存放。 氢化催化剂。氢化苯环,使胺与b-酮酸合成a-氨基酸等。
用途
氢化催化剂。氢化苯环,使胺与b-酮酸合成a-氨基酸等。
30g氯化钯溶于43ml浓盐酸和570ml水中,加入68.6g活性炭,迅速搅拌并加热至60℃。在此混合物中加入31g粒状氢氧化钠,加入的速度以温度不超过80℃为宜。然后在混合物中加入6.6g固体碳酸氢钠,搅拌12h。滤出催化剂,用430ml水洗涤,再用430ml水和8.6ml乙酸的混合液洗涤。滤出催化剂,在65℃真空下干燥。在N2保护下存放。 氢化催化剂。氢化苯环,使胺与b-酮酸合成a-氨基酸等。
用途
氢化催化剂。氢化苯环,使胺与b-酮酸合成a-氨基酸等。